Our eternal pursuits are the attitude of "regard the market, regard the custom, regard the science" and the theory of "quality the basic, trust the first and management the advanced" for Viton Rubber Properties, Vc30, Fkm Base Polymer, We maintain timely delivery schedules, impressive designs, high-quality and transparency for our buyers. Our moto is to deliver top quality solutions within stipulated time.
Factory Cheap Hot Fkm Epdm Difference - Alkali Steam Resistance FEPM Aflas Compound – FUDI Detail:

Compared to general fluoro rubber, Aflas FEPM has better resistance to alkali and acid. Better electrical insulation and impermeability.

● Hardness: 75 Shore A

● Color: Black, brown

● Application: make O-rings, irregular-shaped rings, gaskets

● Advantage: better resistance to alkali and acid. Better electrical insulation and impermeability.

● Disadvantage: processing is difficult

Technical Data

Items Unit FD4675

Typical Properties

Fluorine Content: % 57
Gravity g/cm3 1.65
Color Black or any other colors

Typical Curing Properties:

Monsanto Moving Die Rheometer 【MDR2000®】100cpm, 0.5°Arc,6 minutes@177℃
ML, Minimum Torque, 0.23 N·m 0.24
MH, Maximum Torque, N·m 0.82
ts2【Time to 2 inch-lb rise from minimum】 2′45″
t90【Time to 90% cure】 4′50″

Typical Physical Properties

Press Cure 10 minutes@170℃Post Cure 5 hours@200℃
Tensile Strength【ASTM D412】 14.5 Mpa 13
Elongation at break【ASTM D412】 % 300
Hardness Shore A【ASTM D 2240) 74
Post Cure 20 hours@200℃
Tensile Strength【ASTM D412】 14.5 Mpa 15.8
Elongation at break【ASTM D412】 % 260
Hardness Shore A【ASTM D 2240) 77
Compression set【ASTM D395 Method B,24h@200℃】 % 15

dbf

Storage

FKM rubber material should be stored in a cool, dry and ventilated place. Shelf life is 12 months since production date.

Package

1. To prevent the compounds stick to each other, we apply PE film between each layer of FKM compounds.

2. Every 5kgs in a transparent PE bag.

3. Every 20kgs/ 25kgs in a carton.

4. 500kgs on a pallet, with strips to reinforce.


Product detail pictures:

Factory Cheap Hot Fkm Epdm Difference - Alkali Steam Resistance FEPM Aflas Compound – FUDI detail pictures

Factory Cheap Hot Fkm Epdm Difference - Alkali Steam Resistance FEPM Aflas Compound – FUDI detail pictures


Related Product Guide:

"Quality first, Honesty as base, Sincere service and mutual profit" is our idea, in order to develop continuously and pursue the excellence for Factory Cheap Hot Fkm Epdm Difference - Alkali Steam Resistance FEPM Aflas Compound – FUDI , The product will supply to all over the world, such as: London, Mexico, Croatia, we are fully determined to control the whole supply chain so as to provide quality products at competitive price in a timely manner. We are keeping up with the advanced techniques, growing through creating more values for our clients and society.
  • The product manager is a very hot and professional person, we have a pleasant conversation, and finally we reached a consensus agreement.
    5 Stars By Karen from Peru - 2018.11.28 16:25
    The sales person is professional and responsible, warm and polite, we had a pleasant conversation and no language barriers on communication.
    5 Stars By Octavia from Mumbai - 2017.05.21 12:31
    Write your message here and send it to us